@@ -16,7 +16,6 @@ Below are some useful material choices. Not all information is provided, but can
|
||||
* G4_BGO: bismuth germanate, an inorganic crystal scintillator with a density of 7.13 g/cm3 and a refractive index of 2.15. Cost 0.8 CHF/cm3
|
||||
* G4_LSO: lutetium oxyorthosilicate, an inorganic crystal scintillator with a density of 7.4 g/cm3 and a refractive index of 1.82. Cost: 6 CHF/cm3
|
||||
* G4_LYSO: lutetium yttrium oxyorthosilicate, an inorganic crystal scintillator with a density of 7.1 g/cm3 and a refractive index of 1.81. 30CHF / cm3
|
||||
* G4_CESIUM_IODIDE: cesium iodide, an inorganic crystal scintillator with a density of 4.51 g/cm3 and a refractive index of 1.79. Cost: basically nothing
|
||||
|
||||
## Absorber materials
|
||||
|
||||
@@ -28,4 +27,5 @@ Below are some useful material choices. Not all information is provided, but can
|
||||
|
||||
## For homogenous calorimeters
|
||||
|
||||
* G4_CESIUM_IODIDE: cesium iodide, an inorganic crystal scintillator with a density of 4.51 g/cm3 and a refractive index of 1.79. Cost: basically nothing
|
||||
* G4_PbWO4: lead tungstate crystal (CMS ECAL). Lead tungstate has a very high density of 19.3 g/cm3 and a very short radiation length of 0.89 cm, which makes it suitable for compact and high-resolution electromagnetic calorimeters. Cost: about 3 CHF/cm3
|
||||
|
||||